XUCHUAN CHEMICAL(SUZHOU) CO., LTD
XUCHUAN CHEMICAL(SUZHOU) CO., LTD
Polyester Polyol and Toluene Diisocyanate Prepolymer
  • Polyester Polyol and Toluene Diisocyanate Prepolymer
  • Polyester Polyol and Toluene Diisocyanate Prepolymer
  • Polyester Polyol and Toluene Diisocyanate Prepolymer
  • Polyester Polyol and Toluene Diisocyanate Prepolymer
  • Polyester Polyol and Toluene Diisocyanate Prepolymer
Polyester Polyol and Toluene Diisocyanate Prepolymer
Polyester Polyol and Toluene Diisocyanate Prepolymer
Polyester Polyol and Toluene Diisocyanate Prepolymer
Polyester Polyol and Toluene Diisocyanate Prepolymer
Polyester Polyol and Toluene Diisocyanate Prepolymer

Polyester Polyol and Toluene Diisocyanate Prepolymer

Min. Order:
1000 Kilogram
Min. Order:
1000 Kilogram
Transportation:
Ocean
Port:
Shanghai
Quantity:

Your message must be between 20 to 2000 characters

Contact Now
Basic Info
Basic Info
Place of Origin: China
Productivity: 250000MT/year
Supply Ability: 250000 tons/year
Payment Type: L/C,T/T,D/P
Incoterm: FOB,CFR,CIF
HS Code: 39095000
Transportation: Ocean
Port: Shanghai
Product Description
Product Description


Product Description

Cpu For Elastomers


Polyester Polyol and Toluene Diisocyanate Prepolymer

Polyether Polyurethane Prepolymer

POLYSETER PREPOLYMER  XCPU-E843S

1,This product is a polyester polyol and toluene diisocyanate (T-80) in the

 synthesis of polyester polyurethane prepolymer

2,Features: excellent wear resistance, oil resistance, mechanical properties

3,Uses: Sieve, machinery parts, sealing ring, PU roller and other products

4,Typical propertties of PU matrix:

Name of products

Appearances

Viscosity(mPa.s/85)

NCO% content

Package(kg)

XCPU-E843S

solid

2000-2200

4.30-4.50

20 / 200

5,Operating procedures:

Prepolymer at 80 ~ 85  preheating, after vacuum degassing, the melt TMP 

good homogeneous mixing, deaeration, pouring, molding, vulcanization molding, 

stripping, vulcanization.

6,Reactioon parameter and physical properties:


Article Number

XCPU-E843S

Prepolymer/ g

100

100

100

100

100

Plasticizer /g

0

20

40

50

60

TMP/g

4.3

4.3

4.3

4.3

4.3

Pot Life (adjustable)

0.5~2h

Post Cure Time /(h/℃)

16/100

16/100

16/100

16/100

16/100

Temperature/℃(Prepolymer /TMP)

90/90

90/90

90/90

90/90

90/90

Hardness(Shore A)

60

50

40

35

30

Tensile Strength /MPa

20

15

6

5

3

Elongation / %

500~600

Angle Tear Strength, Die C /(KN/m)

25

20

15

13

10

Resilience (25)/ %

20

40

58

60

60

Gravity (25℃)/(g/ cm3)

1.22~1.27